Deck 27: Weldability of Metals

Full screen (f)
exit full mode
Question
In the steel classification system, the last two digits refer to ____.

A) the basic type of steel
B) the range of carbon content
C) the melting point
D) the basic alloy group
Use Space or
up arrow
down arrow
to flip the card.
Question
For steels containing more than ____ % carbon, preheating and subsequent heat treatment generally are required.

A) 0.30
B) 0.40
C) 30
D) 40
Question
High carbon steels usually have a carbon content of ____ %.

A) 0.30
B) 0.30 to 0.50
C) 0.50 to 0.90
D) 30 to 90
Question
The carbon content of high manganese steel is ____ %.

A) 0.01 to 0.14
B) 0.30 to 0.50
C) 0.50 to 0.90
D) 1 to 1.4
Question
Steel is classified according to ____.

A) melting point
B) ductility
C) basic chemical composition
D) hardness
Question
The strength of ____ stainless steels is the result of a special heat treatment.

A) ferritic
B) austenitic
C) martensitic
D) precipitation hardening
Question
If the chromium-nickel content of a stainless steel is referred to as 25-12, then it contains ____.

A) 25 percent nickel and 12 percent chromium
B) 75 percent chromium and 8 percent nickel
C) 25 percent chromium and 12 percent nickel
D) 75 percent nickel and 8 percent chromium
Question
Most welding processes produce a(n) ____ in which the metals are heated over a range of temperatures.

A) thermal cycle
B) fusion cycle
C) interpass temperature
D) phase change
Question
In both steel classification systems, the first number often, but not always, refers to ____.

A) the most appropriate type of welding
B) the basic type of steel
C) the melting point
D) the carbon content
Question
Low carbon steel has a carbon content of less than ____ %.

A) 0.15
B) 0.30
C) 0.50
D) 30
Question
To improve weldability in stainless steel, the carbon content should not be more than ____ %.

A) 0.03
B) 0.30
C) 3.0
D) 30.0
Question
High manganese steel contains ____ % or more manganese.

A) 0.12
B) 0.22
C) 12
D) 22
Question
____ stainless steels are used for ornamental or decorative applications such as architectural trim, and tend to be brittle.

A) Ferritic
B) Austenitic
C) Martensitic
D) Precipitation hardening
Question
Medium carbon steel has ____ % carbon content.

A) 0.30
B) 0.30 to 0.50
C) 30
D) 30 to 50
Question
The ability of carbon steel to be welded is a function of ____.

A) the melting point
B) the ductility
C) the welding process
D) the carbon content
Question
Chromium carbides form when the metal is between ____ Fahrenheit.

A) 200° and 500º
B) 500° and 800º
C) 800° and 1500°
D) 1500° and 2000°
Question
In the AISI system, the letter ____ indicates basic open-hearth or electric furnace steel and basic oxygen furnace steel.

A) C
B) E
C) F
D) O
Question
____ stainless steels are used in applications requiring both wear resistance and corrosion resistance, such as surgical knives and razor blades.

A) Ferritic
B) Austenitic
C) Martensitic
D) Precipitation hardening
Question
When welding tool steel using the gas welding method, the rods selected for welding repairs should have ____.

A) a carbon content matching the base metal
B) a much higher carbon content than the base metal
C) a slightly higher carbon content than the base metal
D) a much lower carbon content than the base metal
Question
Which of the following is a stainless steel alloy group?

A) Chromium alloy
B) Nickel chromium
C) Manganese alloy
D) Ferritic
Question
​What is the major purpose of pre- and post-heating cast iron for welding?

A) ​To allow the weld to fuse deeper into the joint.
B) ​To control the rate of temperature change.
C) ​To reduce the carbon content in the casting around the weld which makes it less brittle.
D) ​It helps the weld metal flow more evenly into the crack.
Question
____________________ steel is used for wear resistance in applications involving impact, such as power shovels, rock crushers, mine equipment, and augers.
Question
​Why must some castings be repaired without pre- and post-heating?

A) ​They are large or have to be repaired in place.
B) ​They are made of a type of cast iron that cannot be preheated because it is too soft.
C) ​It would damage the paint job on the part.
D) ​Cast iron repairs always require pre- and post-heating.
Question
​Why are fluxing materials used for welding?

A) ​To produce a shinier surface on the weld.
B) ​Because some metals are reactive to the atmosphere when heated.
C) ​It is a way to help control the heat input to the base plate.
D) ​To insure 100% joint penetration on V-grooved joints.
Question
Pure aluminum melts at ____ Fahrenheit.

A) 1200°
B) 1500°
C) 1800°
D) 2200°
Question
All five types of cast iron have carbon contents ranging from ____ %.

A) 0.30 to 0.50
B) 0.50 to 0.90
C) 1.7 to 2
D) 1.7 to 4
Question
​Chromium-molybdenum steel welds have a tensile strength of ____ psi.

A) ​10,000 to 25,000
B) ​30,000 to 45,000
C) ​60,000 to 80,000
D) ​90,000 to 100,000
Question
____________________ steels contain specified larger proportions of alloying elements.
Question
​Why must metal that is below 70°F (20°C) be preheated before welding?

A) ​If the metal is too cold, you cannot get a weld pool established.
B) ​Because the cold metal quenches the weld.
C) ​The arc on cold metal is not stable, and it will wander around the surface making it hard to keep the weld going along the joint.
D) ​The hot metal on the cold plate will not stick, it just bounces off.
Question
​Why must all surface contamination be removed before making a repair weld?

A) ​To prevent injuring your health from exposure to materials released during welding.
B) ​Some chemicals contaminations can be completely safe until they are exposed to the welding.
C) ​The smoke or fumes contamination produce can be an irritant to the skin or eyes.
D) ​All of the above
Question
Steels alloyed with carbon and a low concentration of silicon and manganese are known as ____________________ steels.
Question
​Which type of cast iron undergoes a transformation as a result of a long heat-treating process to reduce hardness?

A) ​gray
B) ​white
C) ​malleable
D) ​nodular
Question
​What type of flux is required to gas weld cast iron?

A) ​C-flux
B) ​Acid flux
C) ​High temperature cast iron welding flux.
D) ​No flux is required to gas weld cast iron.
Question
​____ stainless steels tend to be brittle unless specially deoxidized.

A) ​Ferritic
B) ​Austenitic
C) ​Martensitic
D) ​Precipitation hardening
Question
____________________ steel has a carbon content of 0.8% to 1.5%, making it very difficult to weld.
Question
The weight of magnesium is ____ that of steel, and ____ that of aluminum.

A) 1/4, 1/2
B) 1/4, 2/3
C) 1/3, 2/3
D) 1/2, 2/3
Question
The term ____________________ describes the ease with which a metal can be welded properly.
Question
​Which type of cast iron is the most widely used?

A) ​gray
B) ​white
C) ​malleable
D) ​alloy
Question
​Which of the following is not a common defect if the wrong filler metal is selected for a weld?

A) ​porosity
B) ​cracks
C) ​underfill
D) ​Filler metal just will not stick.
Question
​What is the most common preheating temperature range for most steels?

A) ​250°F to 400°F (120°C to 200°C)
B) ​50°F to 100°F (10°C to 37°C)
C) ​350°F to 650°F (170°C to 340°C)
D) ​65°F to 145°F (18°C to 62°C)
Question
Two of the most important properties of the nonferrous metal ____________________ are its extremely high strength-to-weight ratio (in alloy form) and its generally excellent corrosion resistance.
Question
____________________ stainless steels contain almost no nickel and are cheaper than austenitic steels.
Question
Explain the meaning of the numbers in the SAE and AISI classification systems.
Question
Describe the two recommended procedures to be observed for arc welding tool steel.
Question
The most widely used stainless steels are the ____________________ types.
Question
How can cracks in martensite be prevented?
Question
____________________ steels are used because of increasing demand for high strength and less weight.
Question
Chromium and carbon combine to form ____________________.
Question
Explain why a part must be cleaned before repair or maintenance welding can be performed.
Question
Summarize the uses of chromium-molybdenum steel, including applications it is used for, processes used to weld it, and its tensile strength.
Unlock Deck
Sign up to unlock the cards in this deck!
Unlock Deck
Unlock Deck
1/50
auto play flashcards
Play
simple tutorial
Full screen (f)
exit full mode
Deck 27: Weldability of Metals
1
In the steel classification system, the last two digits refer to ____.

A) the basic type of steel
B) the range of carbon content
C) the melting point
D) the basic alloy group
B
2
For steels containing more than ____ % carbon, preheating and subsequent heat treatment generally are required.

A) 0.30
B) 0.40
C) 30
D) 40
B
3
High carbon steels usually have a carbon content of ____ %.

A) 0.30
B) 0.30 to 0.50
C) 0.50 to 0.90
D) 30 to 90
C
4
The carbon content of high manganese steel is ____ %.

A) 0.01 to 0.14
B) 0.30 to 0.50
C) 0.50 to 0.90
D) 1 to 1.4
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
5
Steel is classified according to ____.

A) melting point
B) ductility
C) basic chemical composition
D) hardness
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
6
The strength of ____ stainless steels is the result of a special heat treatment.

A) ferritic
B) austenitic
C) martensitic
D) precipitation hardening
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
7
If the chromium-nickel content of a stainless steel is referred to as 25-12, then it contains ____.

A) 25 percent nickel and 12 percent chromium
B) 75 percent chromium and 8 percent nickel
C) 25 percent chromium and 12 percent nickel
D) 75 percent nickel and 8 percent chromium
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
8
Most welding processes produce a(n) ____ in which the metals are heated over a range of temperatures.

A) thermal cycle
B) fusion cycle
C) interpass temperature
D) phase change
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
9
In both steel classification systems, the first number often, but not always, refers to ____.

A) the most appropriate type of welding
B) the basic type of steel
C) the melting point
D) the carbon content
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
10
Low carbon steel has a carbon content of less than ____ %.

A) 0.15
B) 0.30
C) 0.50
D) 30
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
11
To improve weldability in stainless steel, the carbon content should not be more than ____ %.

A) 0.03
B) 0.30
C) 3.0
D) 30.0
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
12
High manganese steel contains ____ % or more manganese.

A) 0.12
B) 0.22
C) 12
D) 22
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
13
____ stainless steels are used for ornamental or decorative applications such as architectural trim, and tend to be brittle.

A) Ferritic
B) Austenitic
C) Martensitic
D) Precipitation hardening
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
14
Medium carbon steel has ____ % carbon content.

A) 0.30
B) 0.30 to 0.50
C) 30
D) 30 to 50
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
15
The ability of carbon steel to be welded is a function of ____.

A) the melting point
B) the ductility
C) the welding process
D) the carbon content
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
16
Chromium carbides form when the metal is between ____ Fahrenheit.

A) 200° and 500º
B) 500° and 800º
C) 800° and 1500°
D) 1500° and 2000°
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
17
In the AISI system, the letter ____ indicates basic open-hearth or electric furnace steel and basic oxygen furnace steel.

A) C
B) E
C) F
D) O
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
18
____ stainless steels are used in applications requiring both wear resistance and corrosion resistance, such as surgical knives and razor blades.

A) Ferritic
B) Austenitic
C) Martensitic
D) Precipitation hardening
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
19
When welding tool steel using the gas welding method, the rods selected for welding repairs should have ____.

A) a carbon content matching the base metal
B) a much higher carbon content than the base metal
C) a slightly higher carbon content than the base metal
D) a much lower carbon content than the base metal
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
20
Which of the following is a stainless steel alloy group?

A) Chromium alloy
B) Nickel chromium
C) Manganese alloy
D) Ferritic
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
21
​What is the major purpose of pre- and post-heating cast iron for welding?

A) ​To allow the weld to fuse deeper into the joint.
B) ​To control the rate of temperature change.
C) ​To reduce the carbon content in the casting around the weld which makes it less brittle.
D) ​It helps the weld metal flow more evenly into the crack.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
22
____________________ steel is used for wear resistance in applications involving impact, such as power shovels, rock crushers, mine equipment, and augers.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
23
​Why must some castings be repaired without pre- and post-heating?

A) ​They are large or have to be repaired in place.
B) ​They are made of a type of cast iron that cannot be preheated because it is too soft.
C) ​It would damage the paint job on the part.
D) ​Cast iron repairs always require pre- and post-heating.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
24
​Why are fluxing materials used for welding?

A) ​To produce a shinier surface on the weld.
B) ​Because some metals are reactive to the atmosphere when heated.
C) ​It is a way to help control the heat input to the base plate.
D) ​To insure 100% joint penetration on V-grooved joints.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
25
Pure aluminum melts at ____ Fahrenheit.

A) 1200°
B) 1500°
C) 1800°
D) 2200°
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
26
All five types of cast iron have carbon contents ranging from ____ %.

A) 0.30 to 0.50
B) 0.50 to 0.90
C) 1.7 to 2
D) 1.7 to 4
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
27
​Chromium-molybdenum steel welds have a tensile strength of ____ psi.

A) ​10,000 to 25,000
B) ​30,000 to 45,000
C) ​60,000 to 80,000
D) ​90,000 to 100,000
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
28
____________________ steels contain specified larger proportions of alloying elements.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
29
​Why must metal that is below 70°F (20°C) be preheated before welding?

A) ​If the metal is too cold, you cannot get a weld pool established.
B) ​Because the cold metal quenches the weld.
C) ​The arc on cold metal is not stable, and it will wander around the surface making it hard to keep the weld going along the joint.
D) ​The hot metal on the cold plate will not stick, it just bounces off.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
30
​Why must all surface contamination be removed before making a repair weld?

A) ​To prevent injuring your health from exposure to materials released during welding.
B) ​Some chemicals contaminations can be completely safe until they are exposed to the welding.
C) ​The smoke or fumes contamination produce can be an irritant to the skin or eyes.
D) ​All of the above
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
31
Steels alloyed with carbon and a low concentration of silicon and manganese are known as ____________________ steels.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
32
​Which type of cast iron undergoes a transformation as a result of a long heat-treating process to reduce hardness?

A) ​gray
B) ​white
C) ​malleable
D) ​nodular
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
33
​What type of flux is required to gas weld cast iron?

A) ​C-flux
B) ​Acid flux
C) ​High temperature cast iron welding flux.
D) ​No flux is required to gas weld cast iron.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
34
​____ stainless steels tend to be brittle unless specially deoxidized.

A) ​Ferritic
B) ​Austenitic
C) ​Martensitic
D) ​Precipitation hardening
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
35
____________________ steel has a carbon content of 0.8% to 1.5%, making it very difficult to weld.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
36
The weight of magnesium is ____ that of steel, and ____ that of aluminum.

A) 1/4, 1/2
B) 1/4, 2/3
C) 1/3, 2/3
D) 1/2, 2/3
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
37
The term ____________________ describes the ease with which a metal can be welded properly.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
38
​Which type of cast iron is the most widely used?

A) ​gray
B) ​white
C) ​malleable
D) ​alloy
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
39
​Which of the following is not a common defect if the wrong filler metal is selected for a weld?

A) ​porosity
B) ​cracks
C) ​underfill
D) ​Filler metal just will not stick.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
40
​What is the most common preheating temperature range for most steels?

A) ​250°F to 400°F (120°C to 200°C)
B) ​50°F to 100°F (10°C to 37°C)
C) ​350°F to 650°F (170°C to 340°C)
D) ​65°F to 145°F (18°C to 62°C)
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
41
Two of the most important properties of the nonferrous metal ____________________ are its extremely high strength-to-weight ratio (in alloy form) and its generally excellent corrosion resistance.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
42
____________________ stainless steels contain almost no nickel and are cheaper than austenitic steels.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
43
Explain the meaning of the numbers in the SAE and AISI classification systems.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
44
Describe the two recommended procedures to be observed for arc welding tool steel.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
45
The most widely used stainless steels are the ____________________ types.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
46
How can cracks in martensite be prevented?
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
47
____________________ steels are used because of increasing demand for high strength and less weight.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
48
Chromium and carbon combine to form ____________________.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
49
Explain why a part must be cleaned before repair or maintenance welding can be performed.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
50
Summarize the uses of chromium-molybdenum steel, including applications it is used for, processes used to weld it, and its tensile strength.
Unlock Deck
Unlock for access to all 50 flashcards in this deck.
Unlock Deck
k this deck
locked card icon
Unlock Deck
Unlock for access to all 50 flashcards in this deck.